Electrospun porous cellulose acetate fibers from volatile solvent mixture

buir.contributor.orcidUyar, Tamer|0000-0002-3989-4481
dc.citation.epage2294en_US
dc.citation.issueNumber14en_US
dc.citation.spage2291en_US
dc.citation.volumeNumber65en_US
dc.contributor.authorÇelebioğlu, Aslıen_US
dc.contributor.authorUyar, Tameren_US
dc.date.accessioned2016-02-08T09:51:56Z
dc.date.available2016-02-08T09:51:56Z
dc.date.issued2011en_US
dc.departmentInstitute of Materials Science and Nanotechnology (UNAM)en_US
dc.description.abstractElectrospun porous cellulose acetate (CA) fibers were produced from highly volatile binary solvent system; dichloromethane(DCM)/acetone. The morphology and porous structure of CA fibers were highly dependent on DCM/acetone ratio and the concentration of the solutions. Ribbon-like porous CA fibers were obtained from 5% (w/v) to 10% (w/v) polymer solutions depending on the DCM/acetone ratio; 1/1, 2/1, 3/1 and 9/1 (v/v). Using higher DCM/acetone ratio resulted in bead-free fibers from less concentrated polymer solutions due to the high viscosity of the solutions, in addition, more porous CA fibers were obtained owing to the high volatility of DCM.en_US
dc.identifier.doi10.1016/j.matlet.2011.04.039en_US
dc.identifier.issn0167-577X
dc.identifier.urihttp://hdl.handle.net/11693/21850
dc.language.isoEnglishen_US
dc.publisherElsevieren_US
dc.relation.isversionofhttp://dx.doi.org/10.1016/j.matlet.2011.04.039en_US
dc.source.titleMaterials Lettersen_US
dc.subjectCellulose acetateen_US
dc.subjectElectrospinningen_US
dc.subjectNanofiberen_US
dc.subjectPorousen_US
dc.subjectRibbon-likeen_US
dc.titleElectrospun porous cellulose acetate fibers from volatile solvent mixtureen_US
dc.typeArticleen_US

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Electrospun porous cellulose acetate fibers from volatile solvent mixture.pdf
Size:
701.44 KB
Format:
Adobe Portable Document Format
Description:
Full printable version