Fabrication of mesoporous nickel pyrophosphate electrodes and their transformation to nickel hydroxide with decent capacitance in alkaline media

buir.contributor.authorUlu, Işıl
buir.contributor.authorUlgut, Burak
buir.contributor.authorDağ, Ömer
buir.contributor.orcidUlgut, Burak|0000-0002-4402-0033
buir.contributor.orcidDağ, Ömer|0000-0002-1129-3246
dc.citation.epage22395en_US
dc.citation.issueNumber41
dc.citation.spage22384
dc.citation.volumeNumber11
dc.contributor.authorUlu, Işıl
dc.contributor.authorUlgut, Burak
dc.contributor.authorDağ, Ömer
dc.date.accessioned2024-03-14T09:27:57Z
dc.date.available2024-03-14T09:27:57Z
dc.date.issued2023-10-09
dc.departmentDepartment of Chemistry
dc.description.abstractThe development of high-energy-density electrodes is paramount for the advancement of renewable and clean energy storage materials. In this study, we have devised a synthetic approach to fabricate mesoporous Ni2P2O7 (m-NiPP) electrodes with a decent charge capacity. The method involves the formation of a liquid crystalline mesophase from an aqueous solution containing nickel nitrate hexahydrate salt (Ni(II)), pyrophosphoric acid (PPA), and a non-ionic surfactant (P123). The mesophase solidifies through the polymerization of Ni(II) ions and PPA, ultimately forming a mesostructured Ni2HxP2O7(NO3)x·nH2O semi-solid, which can be subsequently calcined to yield mesoporous Ni2P2O7 (m-NiPP). The gelation and polymerization process can be monitored using gravimetric, ATR-FTIR, XRD, and POM techniques as water evaporates during the transformation. The results reveal that the reaction between the Ni(II) ion and PPA initiates in the solution phase, continues in the gel phase, and concludes upon gentle heating. The same clear aqueous solution can be coated onto a substrate, such as FTO or graphite rods, and then calcined at various temperatures to produce the m-NiPP electrodes, composed of spherical mesoporous NiPP particles. These electrodes remain amorphous over a wide temperature range, but crystallize at approximately 700 °C while retaining their porous structure. However, when exposed to a 3 M KOH solution, the spherical m-NiPP particles undergo a transformation into β-Ni(OH)2 particles. These transformed particles are approximately 1.5 nm thick, equivalent to 3–4 layers, and 7 nm wide, all while maintaining their spherical morphology. This transformation process occurs rapidly for amorphous m-NiPP and proceeds more slowly in the case of crystalline m-NiPP. The resulting electrodes exhibit a substantial charge capacity of 422 C g−1 and an impressive specific capacitance of over 1407 F g−1.
dc.description.provenanceMade available in DSpace on 2024-03-14T09:27:57Z (GMT). No. of bitstreams: 1 Fabrication-of-mesoporous-nickel-pyrophosphate-electrodes-and-their-transformation-to-nickel-hydroxide-with-decent-capacitance-in-alkaline-mediaJournal-of-Materials-Chemistry-A.pdf: 1975337 bytes, checksum: 3a79a9c9a2f57e037bb40f48f7a1c96d (MD5) Previous issue date: 2023-10-09en
dc.identifier.doi10.1039/d3ta05578g
dc.identifier.eissn2050-7496
dc.identifier.issn2050-7488
dc.identifier.urihttps://hdl.handle.net/11693/114733
dc.language.isoen
dc.publisherRoyal Society of Chemistry
dc.relation.isversionofhttps://doi.org/10.1039/d3ta05578g
dc.rightsCC BY
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/
dc.source.titleJournal of Materials Chemistry A: materials for energy and sustainability
dc.titleFabrication of mesoporous nickel pyrophosphate electrodes and their transformation to nickel hydroxide with decent capacitance in alkaline media
dc.typeArticle

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Fabrication_of_mesoporous_nickel_pyrophosphate_electrodes_and_their_transformation_to_nickel_hydroxide_with_decent_capacitance_in_alkaline_media
Size:
1.88 MB
Format:
Adobe Portable Document Format

License bundle

Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
2.01 KB
Format:
Item-specific license agreed upon to submission
Description: