Çelebioğlu, AslıUyar, Tamer2016-02-082016-02-0820110167-577Xhttp://hdl.handle.net/11693/21850Electrospun porous cellulose acetate (CA) fibers were produced from highly volatile binary solvent system; dichloromethane(DCM)/acetone. The morphology and porous structure of CA fibers were highly dependent on DCM/acetone ratio and the concentration of the solutions. Ribbon-like porous CA fibers were obtained from 5% (w/v) to 10% (w/v) polymer solutions depending on the DCM/acetone ratio; 1/1, 2/1, 3/1 and 9/1 (v/v). Using higher DCM/acetone ratio resulted in bead-free fibers from less concentrated polymer solutions due to the high viscosity of the solutions, in addition, more porous CA fibers were obtained owing to the high volatility of DCM.EnglishCellulose acetateElectrospinningNanofiberPorousRibbon-likeElectrospun porous cellulose acetate fibers from volatile solvent mixtureArticle10.1016/j.matlet.2011.04.039