Lecaplain, C.Ortac, BülendMacHinet G.Boullet J.Baumgartl, M.Schreiber, T.Cormier, E.Hideur, A.2016-02-082016-02-082011http://hdl.handle.net/11693/28351Date of Conference: 22-26 May 2011Energy scaling of ultrafast Yb-doped fiber oscillators has experienced rapid progress largely driven by many applications that require high average power femtosecond pulses. The fundamental challenge for ultrafast fiber lasers relies on the control of excessive nonlinearity, which limits pulse energy. The development of all-normal dispersion laser cavities based on large-mode-area photonic crystal fibers (PCFs) has enabled significant energy scaling [1-3]. In particular, up to microjoule energy levels have been achieved from rod-type fiber-based oscillators [2-3]. In such lasers, pulse shaping is dominated by the strength of the mode-locking mechanism which determines the pulse properties. In this contribution, we report the generation of high-energy sub-picosecond pulses from a highly normal dispersion fiber laser featuring an Yb-doped rod-type PCF and a large-mode-area PCF [Fig.1(a)]. Passive mode-locking is achieved using saturable absorber mirrors (SAMs). We study the influence of the SAM parameters on performances obtained in this new class of fiber oscillators. The structures exhibit 20 % modulation depths and 500 fs relaxation time with resonant and antiresonant designs. The antiresonant SAM structures ensure absorption bandwidths 45 nm while the resonant structures exhibit 20 nm bandwidths. Stable mode locking with average powers as high as 15 μW at 15 MHz repetition rate, corresponding to microjoule energy level are obtained with all the structures. However, pulse properties and pulse shaping mechanism distinguish between resonant and antiresonant designs. Using a broadband antiresonant SAM leads to generation of highly-chirped pulses with 30 ps duration and 10 nm spectral width [Fig.1(b)]. The output pulses are extra-cavity dechirped down to 550 fs duration. By increasing the strength of the mode-locking mechanism through the combination of the SAM with the NPE process, we obtain shorter pulses with slightly boarder spectra. Indeed, the output pulse duration is decreased from 30 ps to 13 ps by adjusting the wave-plates settings. The dechirped pulse duration is then shortened to 450 fs. We note that the current laser performances are limited to 1 J by the available pump power. Using a resonant SAM structure, the output pulse duration is decreased to 7 ps [Fig.1(b)]. This pulse shortening results from the spectral filtering induced by the limited SAM bandwidth. All these results are in good agreement with numerical simulations which will be discussed in this communication. © 2011 IEEE.EnglishAntiresonantEnergy levelEnergy scalingHigh average powerHigh energyLarge-mode-area photonic crystal fibersLaser performanceMicrojouleMode-lockedModelockingModulation depthNon-LinearityNormal dispersionOutput pulsePassive mode lockingPulse durationsPulse energiesPulse shorteningPulse-shapingPump powerRepetition rateResonant structuresSamsSaturable absorber mirrorsSpectral filteringSpectral widthsStable mode lockingUltra-fastUltrafast fiber lasersYb-doped fibersBandwidthDispersion (waves)Electromagnetic pulseElectron opticsFiber lasersFibersMode-locked fiber lasersOpticsPhotonic crystalsPulse shaping circuitsPumping (laser)Quantum electronicsSingle mode fibersUltrashort pulsesYtterbiumPhotonic crystal fibersProperties of a microjoule-class fiber oscillator mode-locked with a SESAMConference Paper10.1109/CLEOE.2011.5942877